Home / Financial Firm (Unknown - Insurer) / Determination 201607
Determination 201607
Storm-damaged boat repainted in enamel - applicant sought full respray in two pack paint
Summary
The applicant's boat was damaged in a storm and repaired by a repairer appointed by the FSP. The applicant disputed the repaint, saying the original two pack paint should have been reapplied, and AFCA determined the FSP was not required to authorise a respray.
The repairer's evidence, supported by two surveyors, showed the original topside paint was single pack enamel, so matching it with enamel was appropriate and the finish met professional marine standards.
Subjects and remedies
natural disasterno remedy
Text of the determination
201607 Determination 1 of 5
DETERMINATION
Case number: 201607
Boat – storm damage – repairs – rectification
SUMMARY OF FACTS
1. The applicant arranged a boat insurance policy with the Financial Services
Provider (FSP) on 20 December 2007. The vessel is 25 years old, 12 metres in
length, 4 metres in beam and a mono hull assembly of timber and fibreglass
construction.
2. On 22 September 2008, the applicant‟s boat was damaged in a storm , and the
applicant lodged a claim with the FSP. On 29 October 2008, the applicant
provided a repair quote from his repairer for an amount of $25,900. The FSP
appointed an independent marine assessing company, (AT) to review the
applicant‟s quote. AT considered the quote excessive and arranged another
repairer (AM) to quote. AM provided a quotation for $15,000 and the FSP
authorised repairs to AM.
3. In December 2008, repairs were completed and the applicant collected his
boat. On 6 January 2009, the applicant advised the FSP that he was unhappy
with the quality of repairs, and in particular the application of hardened enamel
paint rather than a two pack paint on the deck of his boat.
4. The FSP appointed AT to review the applicant‟s concerns. On 26 March 2009,
AT reported that the repairs were satisfactory after obtaining a further report
from a marine repairer. The FSP advised the applicant of its findings, but the
applicant continues to dispute the FSP‟s position, arguing the vessel should be
resprayed in two pack paint.
ISSUE IN DISPUTE
5. Whether the FSP is required to authorise the applicant‟s boat to be respra yed.
RELEVANT POLICY PROVISIONS
“ What we will not pay for (page 19)
We will not pay for:
…
Costs of any part or parts of your boat that wear out
…
A defect in your boat, faulty workmanship, structural defects or faulty design” .
REASONS FOR DECISION
6. I am satisfied that a full exchange of information has taken place between each
party and that each party has had the opportunity to address any issues raised.
The Applicant’s Submission
7. He obtained a quote from his repairer (DM), but the FSP authorised the
repairers to its repairer AM which was five hours away. When he collected the
201607 Determination 2 of 5
boat after repairs, he was not happy with the paint work. The boat was painted
in enamel, but the original paint work was two pack epoxy paint which is more
durable than enamel paint.
8. Despite obtaining expert reports from a marine surveyor and a paint
professional stating the original paint was two pack, the FSP has not agreed to
his concerns, and has supported its repairer who has lied by claiming the
original paint was not two pack epoxy.
The FSP’s Submission
9. After receiving complaints from the applicant, the boat was inspected by the
assessor and by an independent marine surveyor. A report was also obtained
from the FSP‟s marine repairer who repaired the boat. These reports were clear
that the original paint work was a single coat enamel and consequently, a
hardened enamel paint was applied to the vessel once it had been properly
prepared for painting.
10. The assessor, the marine surveyor and the repairer have all agreed that the
quality and finish of the boat was far superior after repairs than it was prior to
the incident that caused the damage.
11. The repairer (AM) paints boats on a regular basis and has been trading for 30
years. In his report he stated:
“... Following a test with polyurethane thinners and subsequent reaction to
thinners in three different patches, we had no option but to sand entire hull
coating undercoat and topcoat by spraying a modified enamel with the addition
of a multi solids hardener. No repairs were obvious after respray and the finish
was far superior to what it was originally ....”
12. An inspection of the cabin exterior indicates that it was painted by hand, with a
brush and roller and the paint was a single coat enamel, not a two pack epoxy
paint. The whole topside of the boat was also painted in a single coat enamel,
and for that reason, the repairs were also completed in enamel.
Consideration of each party’s submission
13. I have reviewed the submissions of the parties in relation to the terms and
conditions of the policy.
14. In this matter, both parties have provided expert reports in support of their
submissions. I have analysed these reports and will comment on them
individually.
15. The applicant is adamant that the boat was painted in two pack epoxy paint and
he has provided two expert reports to support his belief. One report is from a
paint professional, and the second report is from a marine surveyor.
16. On the other hand, the FSP has expert reports from its independent assessor,
the repairer and a marine surveyor, all of whom attest to the fact that the boat
was painted in enamel paint.
17. The applicant‟s marine surveyor has stated in his report dated 16 April 2009:
“.... A single component paint has been applied over the previous two component
coating. The standard of finish appears good but this type of paint is
201607 Determination 3 of 5
considerably less resilient to abrasion, chemical attack and generally less
durable ....”
The surveyor has advised that he inspected the boat six years ago and he
confirmed “... that the vessel was generally in good condition throughout at that
time”.
Whilst I note that the surveyor has stated that the finish „appears good‟, he
does not comment on the paintwork of the cabin. As the topside paintwork is a
significant component of this dispute, I would have expected the surveyor to
make some reference to it being hand painted in enamel. The surveyor has
also mentioned that enamel paint is „generally less durable‟, but h as not
provided any clarification regarding this comment i.e. does that generalisation
apply in this instance, and over what timeframe does the durability of enamel
paint become an issue?
18. The applicant has also provided a supporting document dated 13 May 2009
which is from a local paint expert. In his report, the paint expert states:
“.... The original specification for painting the FRP moulded vessel included a two
component Epoxy Primer and a two component Polyurethane Finish, similar to
our T-325 Epoxy and T-582 Polyurethane Enamel. The owners concern is that
only a single component system was used to refinish the vessel and this is
confirmed by the complete salvation of the new paint by vinyl/acrylic thinners – a
two coat system would be totally resistant to removal. ”
I have concerns in relation to three aspects of this report. Firstly, the expert
refers to the boat as a “moulded vessel” whereas, in fact, it is a mono hull
assembly of timber, coated in fibreglass. Whilst I appreciate this expert is a
technical paint manager, I am not aware whether he is an expert in marine
matters. My second comment relates to his statement regarding the original
specification for the painting of the vessel. He does not clarify the basis for his
knowledge of this 25 year o ld vessel‟s original paint specification. Is that his
assumption based on the owner‟s belief, or is it documented in the vessel‟s
paperwork? I would expect the owner to have provided this documentation if it
existed. My third comment relates to the test that was conducted with the
vinyl/acrylic thinners. We are clearly informed by the FSP and its repairer that
an enamel paint with a multi solid hardener was applied to the boat, so this test
is immaterial to this matter.
19. The FSP has provided three expert reports in support of its submission. The
first report is from the repairer (AM) and is dated 13 July 2009. The repairer
who specialises in boat construction and repairs with 30 years experience, has
advised as follows:
“ On close inspection and following repairs to planking and stringer we observed
as would be common on a vessel of this age and construction a number of
previous paint touch ups.”
“Cabin sides are still in similar condition, i.e. painted in a single pack enamel by
brush and roller in average condition .”
“Following a test with polyurethane thinners and subsequent reaction to thinners
in three different patches, we had no option but to sand entire hull coating
undercoat and topcoat by spraying a modified enamel with the addition of a multi
solids h ardener.”
201607 Determination 4 of 5
“At present the vessel appears to be in good condition for its age, however
[applicant’s name] appears to expect a new for old replacement and after 30
years in this industry it appears he is unique and very hard to please. Vessel was
inspected twice by him prior to removal from our premises and he expressed
satisfaction with the works.”
20. The second report submitted by the FSP is dated 30 July 2009 and is from a
marine surveyor. In his review of the topside paint work, the surveyor stated:
“ On close examination we can confirm that the finish of the topside paint is of
very high quality and definitely up to marine industry standard. ”
In relation to the type of paint applied to the vessel, the surveyor advised:
“ A single pack polyurethane topcoat with a hardening additive will compare
favourably with a 2-pack paint in regards to its UV resistance but may be more
vulnerable to wear and tear due to not being as hard as a 2-pack paint. As
previously stated the quality of finish of the new topside coatings is of
professional industry standard .”
21. The third report submitted by the FSP is dated 14 August 2009 and is from the
independent assessor. In his report he states:
“You will note enclosed is a written response from (repairer AM) dated 13 th July
2009. In particular, upon the question of utilising a single pac paint product, he
states this particular product was utilised with the addition of a multi solid
hardener in order to achieve a quality finish whilst ensuring compatibility with the
product that wa s already on the vessel. In other words, in (repairer’s) opinion,
anything other than the paintwork applied would have resulted in a reaction and
future paint failure. This is because the vessel had pre-existing areas of sub-
standard single pac paint patches from previous repairs which would not allow a
2 pac paint product to be applied to those particular areas.
22. On the basis of these various reports, I am satisfied the repairer who repaired
the applicant‟s boat, is experienced and well qualified in the a rea of boat repairs
and respraying. In preparing the boat for repairs, he tested the existing
paintwork in three different areas and concluded that the existing paintwork was
enamel based, not a two pack epoxy paint. This is further evidenced by the fact
that the cabin has enamel paintwork which has been applied by hand, by brush
and by roller.
23. The quality of the paintwork has been endorsed by both the applicant‟s and the
FSP‟s marine surveyors. Both the FSP‟s surveyor and its assessor have stated
that the new paintwork is up to a professional marine industry standard.
24. Whilst the original paintwork on the vessel may or may not have been a two
pack epoxy finish, no evidence has been presented by the applicant to resolve
that issue.
25. However, I am satisfied that the evidence presented by the repairer is clear and
unambiguous in that the existing paintwork around the damaged areas of the
applicant‟s boat was of a single coat enamel paint. The evidence is also clear
that the cabin of the boat is hand painted in enamel by brush and roller.
CONCLUSION
26. I am satisfied that the repairer has matched the existing paintwork, because to
do otherwise by the use of two pack epoxy paint would risk an adverse
chemical reaction with the old paint and lead to possible future paint failure.
201607 Determination 5 of 5
27. Accordingly, I determine that the paintwork has been completed to a
professional marine industry standard, and the FSP is not required to respray
the applicant‟s boat.
Coded fields were extracted from the text by a language model and may contain errors. The published PDF is the authoritative record.